Abstract:SiCf/SiC ceramic matrix composites exhibit excellent properties such as high specific strength, high-temperature resistance, and corrosion resistance, making them highly promising for aerospace applications. However, SiCf/SiC composites are typically anisotropic and difficult to machine. To address common defects during grinding—such as fiber pull-out, matrix damage, and porosity—a systematic orthogonal test of ultrasonic vibration-assisted grinding was conducted on SiCf/SiC composites using a brazed diamond grinding head. Surface roughness (Sa) was used as the characteristic parameter to evaluate the surface quality of SiCf/SiC composite materials. The results of the orthogonal test were subjected to range analysis and variance analysis. It was found that ultrasonic-assisted grinding can significantly reduce the surface roughness of SiCf/SiC composites and improve surface quality. The results indicate that the degree of influence of the four variable factors on roughness is as follows: cutting depth > feed rate > ultrasonic amplitude > linear velocity. However, the analysis of variance shows that the four factors are independent of each other and that there is no significant difference among them.